CORC

浏览/检索结果: 共26条,第1-10条 帮助

已选(0)清除 条数/页:   排序方式:
Intrinsic stacking fault energy and mechanism for deformation twin formation of solid solution matrix in Ni-based superalloys 期刊论文
Vacuum, 2022, 卷号: 203
作者:  Chen, Jianjun;  Ding, Yutian;  Zhang, Xia;  Gao, Yubi;  Ma, Yuanjun
收藏  |  浏览/下载:22/0  |  提交时间:2022/08/09
Zirconium-enhanced segregation tendency of solutes X and Zr-X co-segregation induced synergistic/antagonistic effects on Ni Σ5 [001](210) grain boundary 期刊论文
Materials Today Communications, 2022, 卷号: 31
作者:  Xue, Hongtao;  Wu, Yaqiao;  Tang, Fuling;  Li, Xiuyan;  Lu, Xuefeng
收藏  |  浏览/下载:31/0  |  提交时间:2022/04/21
Accelerated Design of High gamma ' Solvus Temperature and Yield Strength Cobalt-Based Superalloy Based on Machine Learning and Phase Diagram 期刊论文
FRONTIERS IN MATERIALS, 2022, 卷号: 9, 页码: 9
作者:  Wang, Cuiping;  Chen, Xin;  Chen, Yuechao;  Yu, Jinxin;  Cai, Wensu
收藏  |  浏览/下载:19/0  |  提交时间:2022/07/14
Effect of Ta and Ni on γ′ phase morphology and compression behavior of Co-8.8Al-9.8W superalloys 期刊论文
Materials Science and Engineering A, 2022, 卷号: 839
作者:  Xu, Yangtao;  Lv, Xin;  Ma, Tengfei;  Li, Huai;  Wang, Tongchao
收藏  |  浏览/下载:14/0  |  提交时间:2022/04/21
Solute segregation induced stabilizing and strengthening effects on Ni ς3 [110](111) symmetrical tilt grain boundary in nickel-based superalloys 期刊论文
Journal of Materials Research and Technology, 2021, 卷号: 11, 页码: 1281-1289
作者:  Xue, Hongtao;  Luo, Yaqiao;  Tang, Fuling;  Yu, Xuefeng;  Lu, Xuefeng
收藏  |  浏览/下载:22/0  |  提交时间:2021/06/03
Research Status of Tensile and Compression Deformation Mechanism of Cobalt and Cobalt Based Alloys 期刊论文
Cailiao Daobao/Materials Reports, 2020, 卷号: 34, 期号: 19, 页码: 19117-19121
作者:  Xu, Yangtao;  Wang, Yonghong;  Ma, Hongli
收藏  |  浏览/下载:3/0  |  提交时间:2020/12/18
Research Status of Tensile and Compression Deformation Mechanism of Cobalt and Cobalt Based Alloys 期刊论文
Cailiao Daobao/Materials Reports, 2020, 卷号: 34, 期号: 19, 页码: 19117-19121
作者:  Xu, Yangtao;  Wang, Yonghong;  Ma, Hongli
收藏  |  浏览/下载:2/0  |  提交时间:2022/02/17
Effect of Cr addition on microstructure and welding solidification cracking susceptibility of Co-Al-W based superalloys 期刊论文
JOURNAL OF MANUFACTURING PROCESSES, 2020, 卷号: 56, 页码: 820-829
作者:  Liu, Caiyun;  Sun, Yuan;  Wen, Mingyue;  He, Tong;  Yu, Jinjiang
收藏  |  浏览/下载:12/0  |  提交时间:2021/02/02
Effect of Cr addition on microstructure and welding solidification cracking susceptibility of Co-Al-W based superalloys 期刊论文
JOURNAL OF MANUFACTURING PROCESSES, 2020, 卷号: 56, 页码: 820-829
作者:  Liu, Caiyun;  Sun, Yuan;  Wen, Mingyue;  He, Tong;  Yu, Jinjiang
收藏  |  浏览/下载:16/0  |  提交时间:2021/02/02
Mysterious failure in load-free superalloys under repeated thermal shocks 期刊论文
Acta Materialia, 2020, 卷号: 194, 页码: 276-282
作者:  Wen, Junxia;  Cao, Rui;  Gao, Yanfei
收藏  |  浏览/下载:3/0  |  提交时间:2020/11/14


©版权所有 ©2017 CSpace - Powered by CSpace