Measurement and prediction of vibration displacement in micro-milling of nickel-based superalloy 期刊论文
MEASUREMENT, 2019, 卷号: 145, 页码: 254-263
作者:  Lu, Xiaohong;  Jia, Zhenyuan;  Wang, Xinxin;  Liu, Yubo;  Liu, Mingyang
收藏  |  浏览/下载:24/0  |  提交时间:2019/12/02
The influence factors and prediction of curve surface roughness in micro-milling nickel-based superalloy 会议论文
PROCEEDINGS OF THE ASME 13TH INTERNATIONAL MANUFACTURING SCIENCE AND ENGINEERING CONFERENCE, 2018, VOL 4, 2018-01-01
作者:  Lu, Xiaohong;  Wang, Xinxin;  Sun, Jing;  Zhang, Hong;  Feng, Yixuan
收藏  |  浏览/下载:5/0  |  提交时间:2019/12/02
Cellular Automaton Modeling of Dynamic Recrystallization of Nimonic 80A Superalloy Based on Inhomogeneous Distribution of Dislocations Inside Grains 期刊论文
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2018, 卷号: 27, 页码: 4955-4967
作者:  Xu, Qianhong;  Zhang, Chi;  Zhang, Liwen;  Shen, Wenfei;  Yang, Qing
收藏  |  浏览/下载:10/0  |  提交时间:2019/12/02
Removal of inclusions from nickel-based superalloy by induced directional solidification during electron beam smelting 期刊论文
VACUUM, 2018, 卷号: 156, 页码: 39-47
作者:  You, Qifan;  Yuan, Hua;  Zhao, Longhai;  Li, Jiayan;  You, Xiaogang
收藏  |  浏览/下载:6/0  |  提交时间:2019/12/02
Influence of specimen thickness on the creep behavior of a directional solidification nickel-based superalloy 期刊论文
Vacuum, 2018, 卷号: 150, 页码: 105-115
作者:  Cheng CQ(程从前);  Cao TS(曹铁山);  Zhao J(赵杰)
收藏  |  浏览/下载:4/0  |  提交时间:2019/12/02
Analytical model of work hardening and simulation of the distribution of hardening in micro-milled nickel-based superalloy 期刊论文
INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2018, 卷号: 97, 页码: 3915-3923
作者:  Lu, Xiaohong;  Jia, Zhenyuan;  Yang, Kun;  Shao, Peilin;  Ruan, Feixiang
收藏  |  浏览/下载:4/0  |  提交时间:2019/12/02
The effect of thickness on the creep properties of a single-crystal nickel-based superalloy 期刊论文
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 卷号: 728, 页码: 124-132
作者:  Hu, Yebing;  Zhang, Li;  Cao, Tieshan;  Cheng, Congqian;  Zhao, Pengtao
收藏  |  浏览/下载:13/0  |  提交时间:2019/12/02
Creep-induced microstructural evolution in a nickel-based superalloy designed for advanced ultra-supercritical boilers 期刊论文
MATERIALS CHARACTERIZATION, 2018, 卷号: 139, 页码: 311-318
作者:  Xu, Qingshuang;  Cao, Tieshan;  Ye, Fei;  Xu, Fanghong;  Li, Huifang
收藏  |  浏览/下载:6/0  |  提交时间:2019/12/02
Microstructural Evolution of Oxidation Film on a Single Crystal Nickel-Based Superalloy at 980 A degrees C 期刊论文
OXIDATION OF METALS, 2018, 卷号: 89, 页码: 303-317
作者:  Hu, Yebing;  Cheng, Congqian;  Zhang, Li;  Cao, Tieshan;  Guo, Guangping
收藏  |  浏览/下载:12/0  |  提交时间:2019/12/02
Microstructure characteristic and mechanical property of pulsed laser lap-welded nickel-based superalloy and stainless steel 期刊论文
JOURNAL OF MANUFACTURING PROCESSES, 2017, 卷号: 25, 页码: 220-226
作者:  Zhou, Siyu;  Chai, Dongsheng;  Yu, Jingling;  Ma, Guangyi;  Wu, Dongjiang
收藏  |  浏览/下载:3/0  |  提交时间:2019/12/02