Preparing activated carbon by activating molten salt comprises crushing the raw material, drying, carrying out pyrolysis reaction, adding generated coke into molten salt, reacting, activating, cooling the product, and drying. 专利
申请日期: 2014-01-01, 公开日期: 2014-11-26
作者:  GAO N LI A ZHANG L YIN Y
收藏  |  浏览/下载:3/0  |  提交时间:2019/12/11
Preparing activated carbon involves crushing high-carbon material e.g. petrol coke and anthracite, where high-carbon material is mixed with potassium hydroxide to obtain alkali-carbon mixture. 专利
申请日期: 2010-01-01, 公开日期: 2010-05-05
作者:  LI Q LV L XIAO R XU S
收藏  |  浏览/下载:4/0  |  提交时间:2019/12/24
Integrated device for preparing activated carbon, reacts high temperature water steam with semi-coke to generate activated carbon. 专利