Effects of primary Si and applied load on the dry sliding wear behaviors of hypereutectic Al-20Si alloy | |
Li, Qing Lin; Xia, Tian Dong; Lan, Ye Feng; Jian, Yi Sheng | |
2014 | |
会议日期 | November 29, 2013 - November 30, 2013 |
会议地点 | Beijing, China |
关键词 | Aluminum Friction Morphology Silicon Wear of materials Applied loads Dry sliding wear Friction coefficients Morphology and size Primary Si Superheat treatment Wear behaviors Wear properties |
卷号 | 490-491 |
DOI | 10.4028/www.scientific.net/AMM.490-491.83 |
页码 | 83-87 |
英文摘要 | The effects of the primary Si phase and applied load on the dry sliding wear behaviors of hypereutectic Al-20Si alloy were investigated. The results show that coarse polygonal and star-like primary Si was refined into fine blocky shape by increasing superheat treatment temperature. The friction coefficient and wear rate significantly decrease after decreasing the size and changing the morphology of primary Si. Moreover, the friction coefficient and wear rate increase with the increase of applied load. Therefore, the wear properties are greatly influenced by the parameters like morphology and size of primary Si as well as applied load. © (2014) Trans Tech Publications, Switzerland. |
会议录 | Applied Mechanics and Materials |
会议录出版者 | Trans Tech Publications Ltd, Kreuzstrasse 10, Zurich-Durnten, CH-8635, Switzerland |
语种 | 英语 |
ISSN号 | 16609336 |
内容类型 | 会议论文 |
源URL | [http://ir.lut.edu.cn/handle/2XXMBERH/117338] |
专题 | 兰州理工大学 材料科学与工程学院 |
作者单位 | School of Materials Science and Engineering, Lanzhou University of Technology, Lanzhou 730050, China |
推荐引用方式 GB/T 7714 | Li, Qing Lin,Xia, Tian Dong,Lan, Ye Feng,et al. Effects of primary Si and applied load on the dry sliding wear behaviors of hypereutectic Al-20Si alloy[C]. 见:. Beijing, China. November 29, 2013 - November 30, 2013. |
个性服务 |
查看访问统计 |
相关权益政策 |
暂无数据 |
收藏/分享 |
除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。
修改评论