A method for inlet edge hardening of high rating LP stage steam turbine blades usinig temperature controlled high power diode laser hardening process | |
KRISHNARAO VENUGOPAL; VIVEK ARYA; KALYANKAR ARJUN; DITTAKAVI VENKATA VIDYASAGAR | |
2015-11-06 | |
著作权人 | BHARAT HEAVY ELECTRICALS LIMITED |
专利号 | IN396KOL2011A |
国家 | 印度 |
文献子类 | 发明申请 |
其他题名 | A method for inlet edge hardening of high rating LP stage steam turbine blades usinig temperature controlled high power diode laser hardening process |
英文摘要 | The invention relates to a method for inlet edge hardening of LP stage high rating steam turbine blades in a temperature controlled high power diode laser hardening process, comprising : controlling laser power/scan speed to produce droplet erosion resistant hard layer by laser hardening at a temperature in the range of 1400-1700°C and scan speed of 5-2.00 mm to achieve hardness of about 540 HV up to a depth of about 4 mm. |
公开日期 | 2015-11-06 |
申请日期 | 2011-03-24 |
状态 | 未确认 |
内容类型 | 专利 |
源URL | [http://ir.opt.ac.cn/handle/181661/58635] |
专题 | 半导体激光器专利数据库 |
作者单位 | BHARAT HEAVY ELECTRICALS LIMITED |
推荐引用方式 GB/T 7714 | KRISHNARAO VENUGOPAL,VIVEK ARYA,KALYANKAR ARJUN,et al. A method for inlet edge hardening of high rating LP stage steam turbine blades usinig temperature controlled high power diode laser hardening process. IN396KOL2011A. 2015-11-06. |
个性服务 |
查看访问统计 |
相关权益政策 |
暂无数据 |
收藏/分享 |
除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。
修改评论