Corrosion of sintered SiC ceramics in mixed acid solution: temperature and time dependences | |
Liu, Z.[1]; Zhang, H.[2]; Yan, Y.[3]; Wu, H.[4]; Yang, B.[5]; Li, Y.[6]; Liu, X.[7]; Luo, H.[8]; Huang, Z.[9] | |
刊名 | CORROSION ENGINEERING SCIENCE AND TECHNOLOGY |
2017 | |
卷号 | 52页码:38-45 |
关键词 | SiC Acid corrosion Time Temperature |
ISSN号 | 1478-422X |
URL标识 | 查看原文 |
内容类型 | 期刊论文 |
URI标识 | http://www.corc.org.cn/handle/1471x/2193007 |
专题 | 上海大学 |
作者单位 | [1]State Key Laboratory of High Performance Ceramics and Superfine Microstructure, Shanghai Institute of Ceramics, Chinese Academy of Sciences, 1295 Ding xi Road, Shanghai, 200050, China |Department of Materials Science and Engineering, Shanghai University, 99 Shang da Road, Shanghai, 200444, China [2]State Key Laboratory of High Performance Ceramics and Superfine Microstructure, Shanghai Institute of Ceramics, Chinese Academy of Sciences, 1295 Ding xi Road, Shanghai, 200050, China [3]State Key Laboratory of High Performance Ceramics and Superfine Microstructure, Shanghai Institute of Ceramics, Chinese Academy of Sciences, 1295 Ding xi Road, Shanghai, 200050, China [4]State Key Laboratory of High Performance Ceramics and Superfine Microstructure, Shanghai Institute of Ceramics, Chinese Academy of Sciences, 1295 Ding xi Road, Shanghai, 200050, China [5]Key Laboratory of Inorganic Functional Materials and Devices, Shanghai Institute of Ceramics, 1295 Ding xi Road, Shanghai, 200050, China[6]State Key Laboratory of High Performance Ceramics and Superfine Microstructure, Shanghai Institute of Ceramics, Chinese Academy of Sciences, 1295 Ding xi Road, Shanghai, 200050, China [7]State Key Laboratory of High Performance Ceramics and Superfine Microstructure, Shanghai Institute of Ceramics, Chinese Academy of Sciences, 1295 Ding xi Road, Shanghai, 200050, China [8]Department of Materials Science and Engineering, Shanghai University, 99 Shang da Road, Shanghai, 200444, China [9]State Key Laboratory of High Performance Ceramics and Superfine Microstructure, Shanghai Institute of Ceramics, Chinese Academy of Sciences, 1295 Ding xi Road, Shanghai, 200050, China |
推荐引用方式 GB/T 7714 | Liu, Z.[1],Zhang, H.[2],Yan, Y.[3],et al. Corrosion of sintered SiC ceramics in mixed acid solution: temperature and time dependences[J]. CORROSION ENGINEERING SCIENCE AND TECHNOLOGY,2017,52:38-45. |
APA | Liu, Z.[1].,Zhang, H.[2].,Yan, Y.[3].,Wu, H.[4].,Yang, B.[5].,...&Huang, Z.[9].(2017).Corrosion of sintered SiC ceramics in mixed acid solution: temperature and time dependences.CORROSION ENGINEERING SCIENCE AND TECHNOLOGY,52,38-45. |
MLA | Liu, Z.[1],et al."Corrosion of sintered SiC ceramics in mixed acid solution: temperature and time dependences".CORROSION ENGINEERING SCIENCE AND TECHNOLOGY 52(2017):38-45. |